Magnetic transient birefringence of ferrofluids : particle size determination
J.-C. Bacri, R. Perzynski, D. Salin et J. ServaisLaboratoire d'Ultrasons , Université Pierre et Marie Curie, Tour 13, 4, place Jussieu, 75252 Paris, France
Abstract
Relaxation time measurements of magnetically induced birefringence of ferrofluid solutions are performed with samples of various polydispersities. d H, the hydrodynamic diameter of particles deduced from experiments, is compared to a numerical computation with a log-normal distribution. Dynamic magnetic birefringence appears to be a good test of the tail of the sample size distribution. For a narrow distribution (σ ≈ 0.25), the experiment is in good agreement with the model: dH is two times larger than the most probable diameter and corresponds to the largest particles in the sample.
Résumé
Le temps de relaxation de la biréfringence magnétique de solutions de ferrofluide est mesurée pour des échantillons de polydispersité variée. Un diamètre hydrodynamique, dH, des particules est déduit de l'expérience et est comparé à un calcul numérique avec une distribution log-normale. On en déduit que la relaxation de la biréfringence magnétique est une bonne technique pour sonder dans la distribution de taille des échantillons les particules les plus grandes. Lorsque cette distribution est étroite (σ ≈ 0,25 ), l'expérience est en bon accord avec le modèle: dH est deux fois plus grand que le diamètre le plus probable.