Ionic thermocurrent in KCl doped with SO-24

D. Kostopoulos, S. Mourikis et P. Varotsos

Physics Laboratory, University of Athens, Solonos Str. 104, Athens-144, Greece


Abstract
Ionic thermocurrents (ITC) have been measured in crystals of KCl doped with K2SO4. Apart from a small but very wide band at 215 K there are two overlapping bands which have their maxima between 240 and 255 K ; the band maximizing at the higher temperature (246-255 K) is more intense by about one order of magnitude. This intense band corresponds to a migration enthalpy 1.06 ˜ 1.1 eV and a very high preexponential frequency factor 1018 ˜ 1019 s-1 ; the other band seems to have an enthalpy around 0.85 eV and a preexponential factor of the order of 1015 s-1.


Résumé
Les thermocourants ioniques (TCI) ont été mesurés dans des cristaux de KCl dopé avec K2SO4. Excepté pour une petite, mais très large bande à 215 K, on trouve deux bandes se recouvrant dont les maxima sont entre 240 et 255 K ; la bande à la température la plus élevée (246-255 K) est plus intense d'environ un ordre de grandeur. Cette bande intense correspond à une enthalpie de migration de 1,06 ˜ 1,1 eV et à un facteur de fréquence préexponentiel très élevé 1018 ˜ 1019 s-1 . L'autre bande semble avoir une enthalpie de l'ordre de 0,85 eV et un facteur préexponentiel de 1015 s-1 environ.

PACS
6630H - Self-diffusion and ionic conduction in nonmetals.
6630J - Diffusion of impurities.
7722 - Dielectric properties of solids and liquids.

Key words
diffusion in solids -- ionic conduction in solids -- potassium compounds -- sulphur compounds -- thermally stimulated currents