Optical phonon part in spin-lattice relaxation of Cr3+ and Fe3+ ions in rutile
A. Jelennski1, H. Szymczak2 et M. Gutowski21 Institute of Electron Technology, CEMI, Warsaw, Poland
2 Institute of Physics, Polish Academy of Sciences, Warsaw, Poland
Abstract
The results of measurements of EPR line-width at high temperatures (80-450 K) are described for Cr3+ and Fe3+ ions in rutile. These measurements show that at these temperatures spin-lattice relaxation does not depend on the concentration of paramagnetic ions and it is demonstrated that at high temperatures (above 100 K) relaxation in rutile is determined by a Raman process involving optical phonons.
Résumé
On décrit des mesures de largeur de raies en RPE pour des ions Cr 3+ et Fe3+ dans du rutile à températures élevées (80-450 K). Ces mesures montrent qu'à ces températures, la relaxation spin-réseau ne dépend pas de la concentration d'ions paramagnétiques et on établit qu'au-dessus de 100 K, la relaxation dans le rutile est conditionnée par un processus Raman avec participation de phonons optiques.